Abstract
Fine mesh metal powder is produced in a batch or continuous process by reacting a halide vapor with a fine spray of molten sodium below the melting point of the metal. Typically, titanium powder 90% -270 mesh is prepared from ticl4 at 110 deg - 250 deg c.